[1] |
FU H G. Research and application of high speed steel roll [J]. China Molybdenum Industry, 2006, 30(4): 25-32 (in Chinese). |
[2] |
ZHANG X W, LIU H X, JIANG Y H, et al. Laser in situ synthesized TiN/Ti3Al composite coatings [J].Acta Metallurgica Sinica, 2011, 47(8): 1086-1093 (in Chinese). |
[3] |
CHEN Y Y, LI W G, WU P G. In situ synthesis tungsten carbide reinforced ferrous matrix surface composites by laser cladding [J]. Heat Treatment of Metals, 2011, 36(3): 64-67(in Chinese). |
[4] |
ZHANG X W, LIU H X, JIANG Y H, et al. Microstructure of Al2O3/Ti-Al composite coatings prepared by laser aluminum thermal reduction processing [J]. Journal of Inorganic Materials, 2013, 28(9): 1033-1039(in Chinese). |
[5] |
WANG X H, PAN X N, DU B S, et al. Production of in situ TiB2+TiC/Fe composite coating from precursor containing B4C-TiO2-Al powders by laser cladding [J]. Transactions of Nonferrous Metals Society of China, 2013,23(6): 1689-1693. |
[6] |
HE L H, ZHOU F, YANG H Y. Research of in situ synthesis of TiC-TiB2 reinforced Co-based composite coating by laser cladding [J]. Laser Technology, 2013, 37(3): 306-309(in Chinese). |
[7] |
FARID A. Processing, microstructure, properties and wear behavior of in situ synthesized TiB2 and TiC thick films on steel substrates [J]. Surface and Coatings Technology, 2007, 201(24): 9603-9609. |
[8] |
ZHOU F, ZHU T, HE L H. In-situ synthesized TiC-TiB2 composite coatings prepared by laser cladding [J]. China Surface Engineering, 2013, 26(6): 29-34(in Chinese). |
[9] |
JIN Y X, LI Q F. Growth elements and growth habit of coordination polyhedrons of TiC crystal in titanium alloy [J]. Journal of Inorganic Materials, 2004, 19(6): 1249-1254(in Chinese). |
[10] |
GAO W L, ZHANG H, ZHANG E L, et al. Evolution characteristic of primary TiB2 solid-liquid interface morphology in solidification in TiAl-B alloys [J]. Journal of Materials Engineering, 2002(2): 19-22(in Chinese). |
[11] |
YE D L, HU J H. Applied thermodynamic data-sheet of inorganic substances[M]. 2nd ed. Beijing:Metallurgical Industry Press,2002:48 (in Chinese). |
[12] |
ZHU C C, HAO X D, ZHANG X H, et al. Oxidation behavior of TiC-TiB2 multiphase ceramics [J]. Materials Science and Technology, 2004, 12(1): 57-60 (in Chinese). |
[13] |
LI T F. High-temperature oxidation and hot corrosion of metals [M].Beijing:Chemical Industry Press,2003: 52 (in Chinese). |
[14] |
WANG H T, ZHANG G L, YU H S, et al. Effect of chromium, aluminum and silicon on oxidation resistance of Fe-based superalloy [J]. Journal of Materials Engineering, 2008 (12): 73-77 (in Chinese). |