[1] |
FU Y,BATCHELOR A W.Laser nitriding of pure titanium with Ni,Cr for improved wear performance[J].Wear,1998,214(1):83~90. |
[2] |
JIANG P,HE X L,LI X X et al.Wear resistance of a laser surface alloyed Ti-6Al-4Valloy[J].Surf Coat Technol,2000,130(1):24~28. |
[3] |
刘秀波,于利根.王华明. α-TiAl金属间化合物合金激光表面合金化改性[J].稀有金属材料与工程,2001,30(3):224~227. |
[4] |
蒋平,张继娟.Ti-6Al-4V合金激光表面合金化制备Ti5Si3/Ti耐磨复合材料涂层研究[J].稀有金属材料与工程,2000,29(4):269~272. |
[5] |
陈瑶,王华明.TiAl合金激光表面合金层中Ti凝固生长形态及机制[J].中国有色金属学报,2002,12(5):863~868. |
[6] |
何秀丽,王华明,郑启光 et al.TiAl金属间化合物碳元素激光表面合金化[J].金属学报,1998,34(9):983~986. |
[7] |
JACKSON K A. Materials science engineering[M]. New York:McGraw-Hill Book Company,1984.65. |
[8] |
LI R J.Metallic-ceramic composite[M].Beijing:Metallurgy Industrial Press,1995.58~60. |
[9] |
PORTER D A,EASTERLING K E. Phase transformations in metals and alloys[M]. New York:van Nostrand Reinhold,1981.199~203. |
[10] |
胡汉启. 金属凝固[M]. 北京:冶金工业出版社,1985.111~113. |
[11] |
FLEMINGS M C.Solidification processing[M].New York:McGraw-Hill Book Company,1972.126~127. |
[12] |
LIU R P,WANG W K,LI D et al.Transition from continuous to lateral growth for Gecrystal in undercooled Ge74Ni26 alloy melts[J]. Scripta Materialia,1999,41(8):855~860. |